plating surface preparation | |||
Post Reply | Forum |
Posted by: gwood ® 03/29/2005, 16:51:54 Author Profile Mail author Edit |
Hi. Any thoughts would be greatly appreciated on the following:
1) Would placing machined Ti-6Al-4V in a bath of HBF(4)/HCl and then aqueous ultrasonic cleaning present risk for subsequent hydrogen embrittlement or other problems?
Thanks, have a good day.
|