Hi chiefs, I have been asked to do a process feasibility for a nylon bush of 25mm OD and 19mm ID and Length is 35mm. Here we need to achieve +/- 25microns dimensional tolerance at OD and Runout tolerance of 20microns at OD. Material we are going use for this product is 33% Glass filled nylon 66, from dupont. I Spoke to my vendor he said it is not easy to achieve 20 microns rounout tolerance at OD. So please let me know Is this possible to achieve above mentioned tolerance and also let me know what is the minimum runout tolerance i can achieve for the above mentioned case. Thanks in advance, Vijay.G Modified by vijayguru at Wed, Feb 07, 2007, 03:27:01 |
Post Reply Tell a Friend (must be logged in) Alert Admin About Post |
View All | | Next | |
Replies to this message |
Re: Least achievable tolerance in 33% Glass Filled Nylon 66 | |||
Re: Least achievable tolerance in 33% Glass Filled Nylon 66 -- vijayguru | Post Reply | Top of thread | Forum |
Posted by: Marky ® 02/07/2007, 09:06:20 Author Profile eMail author Edit |
I would call Dupont...they'll tell you or recommend another material. In the meantime...buy some material and see what your vendor CAN hold. |
Post Reply Tell a Friend (must be logged in) Alert Admin About Post |
Where am I? Original Top of thread | | | |
Re: Re: Least achievable tolerance in 33% Glass Filled Nylon 66 | |||
Re: Re: Least achievable tolerance in 33% Glass Filled Nylon 66 -- Marky | Post Reply | Top of thread | Forum |
Posted by: vijayguru ® 02/08/2007, 01:25:55 Author Profile eMail author Edit |
Thanks for the effort made by you, awaiting for your feedback....
|
Post Reply Tell a Friend (must be logged in) Alert Admin About Post |
Where am I? Original Top of thread |
Powered by Engineers Edge
© Copyright 2000 - 2024, by Engineers Edge, LLC All rights reserved. Disclaimer