Posted by: martinw ® 01/18/2007, 01:16:12 Author Profile eMail author Edit |
The components we manufacture require a 85 micron thick zinc layer. This is almost impossible to achieve with the nodular iron we make. I have been told that the components need to be decarburised to reduce the exposed carbon on the metal surface. Is this true? Katbos |