Related Resources: materials
Aluminum Alloys Temper designation and subdivisions
Engineering Materials and Specifications
Basic temper designation and subdivisions from aluminum alloys
Basic temper designations and subdivisions from aluminum alloys.
NON HEAT-TREATABLE ALLOYS
|
HEAT-TREATABLE ALLOYS
|
||
Temper Designation
|
Definition
|
Temper Designation
|
Definition
|
-0 | Annealed recrystallized (wrought products only) applies to softest temper of wrought products. | -0 | Annealed recrystallized (wrought products only) applies to softest temper of wrought products. |
-H1 | Strain-hardened only. Applies to products which are strain-hardened to obtain the desired strength without supplementary thermal treatment. | -T1 | Cooled from an elevated temperature shaping process (such as extrusion or casting) and naturally aged to a substantially stable condition. |
-H12 | Strain-hardened one-quarter-hard temper. | -T2 | Annealed (castings only). |
-H14 | Strain-hardened half-hard temper. | -T3 | Solution heat-treated and cold-worked by the flattening or straightening operation. |
-H16 | Strain-hardened three-quarters-hard temper. | -T36 | Solution heat-treated and cold-worked by reduction of 6 percent |
-H18 | Strain-hardened full-hard temper. | -T4 | Solution heat-treated. |
-H2 | Strain-hardened and then partially annealed. Applies to products which are strain-hardened more than the desired final amount and then reduced in strength to the desired level by partial annealing. | -T42 | Solution heat-treated by the user regardless of prior temper (applicable only to 2014 and 2024 alloys). |
-H22 | Strain-hardened and partially annealed to one-quarter-hard temper. | -T5 | Artificially aged only (castings only). |
-H24 | Strain-hardened and partially annealed to half-hard temper. | -T6 | Solution heat-treated and artificially aged. |
-H26 | Strain-hardened and partially annealed to three-quarters-hard temper. | -T62 | Solution heat-treated and aged by user regard-less of prior temper (applicable only to 2014 and 2024 alloys). |
-H28 | Strain-hardened and partially annealed to full-hard temper. | -T351, -T451, -T3510, -T3511, -T4510, -T4511. |
Solution heat-treated and stress relieved by stretching to produce a permanent set of 1 to 3 percent, depending on the product. |
-H3 | Strain-hardened and then stabilized. Applies to products which are strain-hardened and then stabilized by a low temperature heating to slightly lower their strength and increase ductility. | -T651, -T851, -T6510, -T8510, -T6511, -T8511. |
Solution heat-treated, stress relieved by stretch-ing to produce a permanent set of 1 to 3 percent, and artificially aged. |
-H32 | Strain-hardened and then stabilized. Final temper is one-quarter hard. | -T652 | Solution heat-treated, compressed to produce a permanent set and then artificially aged. |
-H34 | Strain-hardened and then stabilized. Final temper is one-half hard. | -T8 | Solution heat-treated, cold-worked and then artificially aged. |
-H36 | Strain-hardened and then stabilized. Final temper is three-quarters hard. | -T/4 | Solution heat-treated, cold-worked by the flattening or straightening operation, and then artificially aged. |
-H38 | Strain-hardened and then stabilized. Final temper is full-hard. | -T86 | Solution heat-treated, cold-worked by reduction of 6 percent, and then artificially aged. |
-H112 | As fabricated; with specified mechanical property limits. | -T9 | Solution heat-treated, artificially aged and then cold-worked. |
-F | For wrought alloys; as fabricated. No mechanical properties limits. For cast alloys; as cast. | -T10 | Cooled from an elevated temperature shaping process artificially aged and then cold-worked. |
-F | For wrought alloys; as fabricated. No mechanical properties limits. For cast alloys; as cast. |
Related: